Overview
We compared incomplete coverage and adhesion early and late in production, including observations before and after pretreatment changes.
We tracked changes in HPPA plating coverage and adhesion at different stages of production. Pretreatment temperature, bath replacement, and trial-plating history were compared with adhesion test results for finished parts.
Some conditions produced fewer small unplated areas and favorable adhesion results. Delamination was observed in initial production parts on other operating days, and these observations were recorded by production stage.