A blackening trial on camera parts at two rack positions
Four polycarbonate (PC) and stainless steel camera parts were plated with electroless nickel on a single rack, then blackened using a treatment from Supplier O.
Plating development, process trials and technical reviews by SUNGJINLOGIS.
73 articles
Four polycarbonate (PC) and stainless steel camera parts were plated with electroless nickel on a single rack, then blackened using a treatment from Supplier O.
The measured quantities in on-site analysis procedures were compared with reporting units in process control tables, and process-specific conversion items were organized.
Fluorine analysis and replenishment records were recalculated using a mass balance, and differences were compared under alternative bath-volume conditions before and after replenishment.
Analysis records for two acid copper tanks at Plant 1 were paired to compare the direction of concentration changes and manual replenishment histories.
Catalyst test records were grouped into single-shot injection molded, conventional two-shot injection molded and special-geometry specimens to define the scope of coverage and selective plating evaluations.
PC pretreatment bath and specimen observations were reclassified, and record fields were designed for a PPS analytical management plan.
Same-day and later evaluations of plated PC were separated from results after subsequent plating stages to compare peeling patterns and the metal layers observed.
Thickness measurements on both sides of plated PPS were reanalyzed by lot, distinguishing average thickness, local deviations and adhesion observations.
Replenishment purposes and replacement histories were linked with working days and throughput to examine differences in pretreatment bath management.
Inspection records for early- and late-run samples were paired to compare dent occurrence and thickness changes in individual metal layers.