Overview
We linked tank deposition observations with cleaning and bath replacement history to track recurrence.
We observed tank conditions before and after production to examine electroless plating bath stability. We tracked when electroless copper deposits appeared and how conditions changed after cleaning, bath disposal, and fresh bath preparation.
We recorded days when tank deposition was absent and days when it reappeared. Bath management and production history were compared for each operating day.