Overview
Inspection records for early- and late-run samples were paired to compare dent occurrence and thickness changes in individual metal layers.
Inspection records for early- and late-run samples from the same date were compared to examine appearance differences with production sequence. Sample groups with recorded dent counts and equal inspection quantities were selected and reviewed separately from staining and adhesion test results.
On the inspection dates compared, more dents were observed in early-run samples than in late-run samples. Copper and nickel thickness measurements on the same inspection sheets were also compared.
On some days, the two metal layers showed opposite directions of thickness change between early- and late-run samples. Appearance results by inspection stage and thickness results by metal layer were organized side by side.